Polymer Property : Shear Strength = 100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 100 MPa

@Temperature 25.0 °C
14500 psi

@Temperature 77.0 °F
Short Beam, Dry
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Information provided by HexCel
Shear Strength 100 MPa

@Temperature 23.0 °C
14500 psi

@Temperature 73.4 °F
In-Plane; prEN6032
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/AS7 GS
Fiber: AS7 GS, UD, 150 g/m2Information provided by HexCel
Shear Strength 100 MPa

@Temperature 23.0 °C
14500 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber
Information provided by HexCel