Polymer Property : Shear Strength = 0.156 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.156 MPa

@Shear Rate 500 1/s,
Temperature 275 °C
22.6 psi

@Shear Rate 500 1/s,
Temperature 527 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..