Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 52200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 360 MPa

@Thickness >=1.60 mm,
Temperature 200 °C
52200 psi

@Thickness >=0.0630 in,
Temperature 392 °F
Perpendicular to laminations; EN 60893
HOS-Technik Homide 250 Bismaleimide Resin
Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel..
Flexural Strength 360 MPa

@Strain 3.00 %
52200 psi

@Strain 3.00 %
ISO 178
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers
PA 6, 50% glass fibers, injection molding, heat-ageing stabilized
Flexural Strength 360 MPa

@Temperature -40.0 °C
52200 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 360 MPa

@Temperature -40.0 °C
52200 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 360 MPa

@Thickness >=1.50 mm
52200 psi

@Thickness >=0.0591 in
1hr/2000°C/measured at 2000°C; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation ..