Mechanical Properties Metric English Comments
Flexural Strength 310 MPa

@Strain 4.00 %
45000 psi

@Strain 4.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 310 MPa

@Temperature -40.0 °C
45000 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.25%); ASTM-D790
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 310 MPa

@Temperature 23.0 °C
45000 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..