Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 260 MPa @Strain 4.00 % |
37700 psi @Strain 4.00 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 260 MPa @Temperature -40.0 °C |
37700 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.25%); ASTM-D790 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 0.8%); ASTM-D790 |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Flexural Strength | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |