Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 13.5 MPa @Temperature 275 °C |
1960 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 13.5 MPa @Temperature 275 °C |
1960 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Flexural Strength | 13.5 MPa @Temperature 275 °C |
1960 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |