Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 77.0 MPa @Temperature 23.0 °C |
11200 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |