Mechanical Properties Metric English Comments
Flexural Strength 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Flexural Strength 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
Flexural Strength 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 90G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Flexural Strength 175 MPa

@Temperature -40.0 °C
25400 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 175 MPa

@Temperature 80.0 °C
25400 psi

@Temperature 176 °F
Practical Use (Water Absorption 1.25%); ASTM-D790
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 175 MPa

@Temperature 80.0 °C
25400 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..