Mechanical Properties Metric English Comments
Flexural Strength 12.0 MPa

@Temperature 275 °C
1740 psi

@Temperature 527 °F
Result based on 450G; ISO 178
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Flexural Strength 12.0 MPa

@Strain 9.00 %
1740 psi

@Strain 9.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 12.0 MPa

@Strain 9.00 %
1740 psi

@Strain 9.00 %
Conditioned; ISO 178
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66  (discontinued **)