Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Arlon A3020-B004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
  1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Prod.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-230A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Warp/Longitudinal direction |
Saint-Gobain Chemlam® 4 Value Industrial Laminate Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass rei.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 500F PTFE Coated Beta Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | silicone property; ASTM D624 |
Arlon 51106R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; Silicone Property; Arlon SQA-TMS-029 |
Arlon 51146R050 0.050" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values for the production materi.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; Silicone Property; ASTM D624 |
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Silicone Property; ASTM D624 |
Arlon 55142R040 0.040" (1.02 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be use.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Silicone Property; ASTM D624 |
Arlon 56146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; Silicone Property; ASTM D624 |
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Silicone Property; ASTM D624 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; Silicone Property; ASTM D624 |
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, layer 2; ASTM D624 |
Arlon 55109R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Silicone Property; ASTM D624 |
Arlon 55146R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sili.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55271R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Interleave 2: Polyethylene Product Use: Flexible heater in.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | [ppiw], Side 2, Silicone Property; ASTM D624 |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
Arlon CP-414R Silicone Rubber bulk compound |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3830E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | die B; ASTM D624 |
R70-057 Styrene-based Biomedical Elastomer |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 44278R018 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEUL.. |
|||
Tear Strength | 15.8 kN/m | 90.0 pli | Die B, Silicone Property; Arlon SQA-TMS-029 |
Arlon 44278R018B 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 1: Cured Silicone RubberInterleave: LDPEUL R.. |