Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 154 kN/m | 880 pli | Die C; ASTM D624 |
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th.. |
|||
Tear Strength | 154 kN/m | 880 pli | ISO 34-1B |
Lubrizol Advanced Materials PEARLTHANE® 11T95P Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T95P is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical p.. |