Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 13.0 kN/m | 74.2 pli | ISO 34-1 |
PolyOne OnFlex™ S KE 40A-3S1727 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Conductive Layer |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Die B |
Momentive Performance Materials FSE7540 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Die B |
Momentive Performance Materials HV 3/406 Heat Cured Rubber - High Temperature Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Die B |
Momentive Performance Materials HV 6/600 Heat Cured Rubber - STEAM Resistant Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 7060 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1522A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Split tear method, MD; ASTM D1938 |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | Split tear method, MD; ASTM D1938 |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | ISO 34-B |
AlphaGary Evoprene™ Super G 946 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
Tear Strength | 13.0 - 30.0 kN/m | 74.2 - 171 pli | ASTM D 624 |
API Megol AM DP2154 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 13.0 kN/m | 74.2 pli | |
Trelleborg Commercial Neoprene® C500 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |