Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 110 kN/m | 630 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-560D Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 110 kN/m | 630 pli | ASTM D624 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |