Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 100 kN/m | 571 pli | Die C; ASTM D624 |
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Tear Strength | 100 kN/m | 571 pli | Injection molded parts; DIN 53515 |
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
GRECO ISOTHANE 2095A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
SPS Guang Zhou POFLEXâ„¢ EP8300 Cable Grade TPU Non-halogen flame-retarded TPU material TPU POFLEXâ„¢ EP8300 is used to produce wire and cable. Halogen-free with good flammability and excellent mechanical property and heat resistance.Informat.. |
|||
Tear Strength | 100 kN/m | 571 pli | DIN 53515 |
Lubrizol ESTANE® T5417 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 100 kN/m | 571 pli | DIN 53515 |
Lubrizol ESTANE® X4985 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 100 kN/m | 571 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-7185 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 100 kN/m | 571 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 100 kN/m | 571 pli | DIN 53515 |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 100 kN/m | 571 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 100 kN/m | 571 pli | DIN 53515 |
Lubrizol ESTANE® 58156 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 100 kN/m | 571 pli | ISO 34 |
Chengdu Polyster H3303B Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and extrusion grade. Contains color-stable antioxidants. Excellent low-temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ boots, hose jack.. |
|||
Tear Strength | 100 kN/m | 571 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tear Strength | 100 kN/m | 571 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tear Strength | 100 kN/m | 571 pli | DIN ISO 34-1/Bb |
BASF Elastollan 695 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 100 kN/m | 571 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 100 kN/m | 571 pli | |
AorTech Biomaterials ECSil™ 90A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tear Strength | 100 kN/m | 571 pli | |
AorTech Biomaterials ECSil™ 90A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tear Strength | 100 kN/m | 571 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
LyondellBasell Hifax™ ETA-3131 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic olefin resin, excellent impact and stiffness balance, excellent processabilityApplications: automotive filler and valance panels, lower a.. |
|||
Tear Strength | 100 kN/m | 571 pli | ASTM D624 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |