Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 10.0 kN/m | 57.1 pli | ISO 34B |
Huntsman AVALON® 550 B Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Insulating Layer |
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Support Rubber |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Insulating Layer |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Insulating Layer |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LIM 6010 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/04 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2530 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 7070 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-10A/B Elastomer KE-1950-10 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | |
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | |
Trelleborg Hypalon® H730 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Split tear method, MD; ASTM D1938 |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® HB5299 PA* Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide.. |
|||
Tear Strength | 10.0 kN/m | 57.1 pli | |
ACC MM903 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |