Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 95.0 kN/m | 542 pli | ISO 34B |
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | |
Huntsman IROGRAN® A 95 K 6977 TPU-For Seals Information provided by Huntsman |
|||
Tear Strength | 95.0 kN/m | 542 pli | ISO 34-1B |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ISO 34B |
Huntsman AVALON® 80 AB Thermoplastic Polyurethane Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ISO 34B |
Huntsman AVALON® 90 AHT DP Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D624 |
GRECO ISOTHANE 1090A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tear Strength | 95.0 kN/m | 542 pli | Die B |
Momentive Performance Materials FQE207U Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D1004 |
SK Chemicals SKYPEL P147D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D1004 |
SK Chemicals SKYPEL G130D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 95.0 kN/m | 542 pli | with incision; ISO 34B |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 95.0 kN/m | 542 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1485RV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 95.0 kN/m | 542 pli | DIN 53515 |
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ISO 34 |
Chengdu Polyster H4040 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance, especially at low temperatures. Moldable even in thin sections. Can be used in light.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | unnotched; ASTM D624 (C) |
Arkema Group Pebax® 4033 Polyether Block Amide (PEBA) Typical application: Mechanical partsInformation provided by Arkema Group |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR8520 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D624 |
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tear Strength | >= 95.0 kN/m | >= 542 pli | ISO 34 |
Austin Novel Materials Texalan® 390A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | >= 95.0 kN/m | >= 542 pli | ISO 34 |
Austin Novel Materials Texalan® 495A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | >= 95.0 kN/m | >= 542 pli | ISO 34 |
Austin Novel Materials Texalan® 585A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tear Strength | >= 95.0 kN/m | >= 542 pli | ISO 34 |
Austin Novel Materials Texalan® 764D PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tear Strength | 95.0 kN/m | 542 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 95.0 kN/m | 542 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | >= 95.0 kN/m | >= 542 pli | ISO 34 |
Austin Novel Materials Texalan® 695A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 95.0 kN/m | 542 pli | with incision; ISO 34B |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |