Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 94.7 kN/m | 540 pli | 73°F; ASTM D624 |
Advanced Elastomer Systems VistaFlex® 911-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tear Strength | 94.6 kN/m | 540 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 94.6 kN/m | 540 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 94.6 kN/m | 540 pli | Die C; ASTM D624 |
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Tear Strength | 94.6 kN/m | 540 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Tear Strength | 94.6 kN/m | 540 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Tear Strength | 94.7 kN/m | 540 pli | Die "C"; ASTM D624 |
DSM Biomedical CarboSil® 10 90A Biocompatible Silicone Polycarbonate Urethane
(discontinued **) Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-En.. |
|||
Tear Strength | 94.7 kN/m | 540 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First Choic.. |
|||
Tear Strength | 94.7 kN/m | 540 pli | ASTM D624 |
Buckeye Polymers BP Flex D4507 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |