Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 81.6 kN/m | 466 pli | ASTM D624 |
Multibase Multi-Flex® TPE D 4308 BLK The moisture content is 0.04%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 81.6 kN/m | 466 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO 4308 BLK Data provided by Multibase. |