Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 67.0 kN/m | 382 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D1938 |
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D1938 |
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D1938 |
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D1938 |
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D1938 |
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D1938 |
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 67.0 kN/m | 382 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D624 |
ELASTO UK Dryflex® 420351S SBS Based Material, 35D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | ASTM D624 |
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 67.0 kN/m | 382 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |