Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 56.0 kN/m | 320 pli | ASTM D624 |
Multibase Multi-Flex® TPE G 7827 GREY Heat aging at 150°C for 7 days results in tensile retention 85% and the elongation retention 75%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 56.0 kN/m | 320 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90451 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 56.0 kN/m | 320 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 56.1 kN/m | 320 pli | ASTM D624 |
Huntsman IROGRAN® PS 456-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Tear Strength | 56.1 kN/m | 320 pli | ASTM D624 |
Multibase Multi-Flex® A 9402 AH Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 56.0 - 71.0 kN/m | 320 - 405 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 14 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Tear Strength | 56.0 - 71.0 kN/m | 320 - 405 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 14G Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |
|||
Tear Strength | 56.1 kN/m | 320 pli | Die C; ASTM D1004 |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 56.1 kN/m | 320 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7100-87 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 56.0 kN/m | 320 pli | Die C; ASTM D624 |
Teknor Apex Uniprene® 87A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
Tear Strength | 56.1 kN/m | 320 pli | Die C; ASTM D624 |
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha.. |
|||
Tear Strength | 56.0 kN/m | 320 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 65A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 56.0 kN/m | 320 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 56.0 kN/m | 320 pli | DIN 53515 |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |
|||
Tear Strength | 56.1 kN/m | 320 pli | |
Cytec EN-7 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tear Strength | 56.1 kN/m | 320 pli | |
Cytec EN-8 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tear Strength | 56.0 kN/m | 320 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 56.0 kN/m | 320 pli | DIN 53515 |
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 56.0 kN/m | 320 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 65A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |