Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 52.5 kN/m | 300 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 9103 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Split; ASTM D624 |
Northstar Polymers MSB-A95A High Performance Polyurethane Cast Elastomer System This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Die C; ASTM D624 |
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Split; ASTM D624 |
Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Tear Strength | 52.5 kN/m | 300 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible K85 Natural & Black Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 52.6 kN/m | 300 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | ASTM D624 |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-270A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 52.6 kN/m | 300 pli | ASTM D624 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Putty, Black Information provided by ITW Devcon |
|||
Tear Strength | 52.6 kN/m | 300 pli | Fill/Transverse direction |
Saint-Gobain COHRlastic® 1025 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Fill/Transverse direction |
Saint-Gobain COHRlastic® 1032 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | |
Saint-Gobain COHRlastic® CF3320 Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 14 Primary PTFE-Coated Glass Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: .. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 3790 Open Mesh Belting Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® TCN® 1590 Leno Weave Nomex/Fiberglass Belting Material Description: General Notes on Saint Gobain Chemfab® TCN® Open Mesh Belting Products:TCN belting products are PTFE coated Nomex®, a high-temperature polyamide fiber that maintains its struct.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Die C; ASTM D624 |
Teknor Apex APEX® 3080-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | |
Saint-Gobain COHRlastic® CF4420 High Heat Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | |
Saint-Gobain COHRlastic® CF4480 High Heat Reversion Resistant Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7010-87 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 52.6 kN/m | 300 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Tear Strength | 52.6 kN/m | 300 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 1589 PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain.. |