Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 45.1 kN/m | 257 pli | post cured- 8 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4765 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 45.1 kN/m | 257 pli | DIN 53515 |
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 70 H 4673 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4673 M is part of the HUNTSMAN injection molding .. |
|||
Tear Strength | 45.1 kN/m | 257 pli | 0.025" extruded film; DIN 53515 |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/60 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | >= 45.0 kN/m | >= 257 pli | DIN 53507 |
Karina 802-06/77-Y-BZ Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4640 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4660 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 70 HS High Strength Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34B |
Huntsman AVALON® 65 AK Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-60A/B Elastomer KEG2000-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | >= 45.0 kN/m | >= 257 pli | |
Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 5702F3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
Trelleborg I644 Antiabrasive SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-990 (MT) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 5702F2 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 58201 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | notched; ASTM D624 (C) |
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN ISO 34-1/Bb |
BASF Elastollan C 75 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
Trelleborg R721 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34-B |
AlphaGary Evoprene™ G 975 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® T5083 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | >= 45.0 kN/m | >= 257 pli | DIN 53507 |
Karina 70/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |