Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 40.0 kN/m | 228 pli | as molded; Die B |
Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 40.0 kN/m | 228 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® C7-4565 DICUP R Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | Method B; ISO 34 |
S&E Specialty Polymers SE900-6 PVC Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Skin which meets the Ford WSKM4D689-A5Information provided by S&E Specialty Polymers |
|||
Tear Strength | 39.9 kN/m | 228 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 39.9 kN/m | 228 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | DIN 53507 |
Karina E CAK 75-48/1 Black PVC Compound Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34B |
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34B |
Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ Electro 242-3 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | DIN 53507 |
Karina 700D40/356-AT Green PVC Compound Non toxic PVC compound, recommended for injection of inhalation maskInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/06 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 50 HS High Strength Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | DIN 53507 |
Karina CAK 75-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94406 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | DIN 53507 |
Karina 70/222 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-50A/B Elastomer KE-1950-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ASTM D2240 |
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 39.9 kN/m | 228 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Trelleborg R798 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 39.9 kN/m | 228 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ASTM D624 |
ELASTO UK Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C; ASTM D624 |
Covestro Bayflex® MP-5000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN ISO 34-1/Bb |
BASF Elastollan C 65 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 50 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN 53515 |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.25 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |