Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 225 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength >= 39.4 kN/m
>= 225 pli
ASTM D624
Multibase Multi-Flex® TPE A 7606 NAT
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 39.4 kN/m
225 pli
ASTM D624
Multibase Multi-Flex® TPE A 8103 BLK
Multi-Flex® A 8103 is a moderately low price TPE that has a god tensile and tear strength as well as very good elasticity. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 39.4 kN/m
225 pli
post cured- 2 hours at 177°C; Die B
Multibase SILASTIC® Q7-4765 Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 39.4 kN/m
225 pli
Split; ASTM D624
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac..
Tear Strength 39.5 kN/m
225 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 39.5 kN/m
225 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 39.5 kN/m
225 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 39.5 kN/m
225 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 39.4 kN/m
225 pli
Fill/Transverse direction
Saint-Gobain Chemlam® Silver 12 Wear Resistant Industrial Laminate
Description: The Chemlam® Silver series is the wear resistant line of Chemfab® industrial laminates. Chemlam® Silver composites feature uniform thickness, multi-layer cast PTFE films lamina..
Tear Strength 39.4 kN/m
225 pli
Fill/Transverse direction
Saint-Gobain Chemlam® XF-900 Fully Sintered PTFE Coated, Flexible, Non-porous Fluoropolymer Laminated Composite
Description: Chemlam® is the trademark for the Chemfab® family of flexible, non-porous fluoropolymer laminated composites that combine the features of multi-layer fluoropolymer cast films with..
Tear Strength 39.4 kN/m
225 pli
Initial Tear Strength
Saint-Gobain CHR® 2905-10R Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°..
Tear Strength 39.4 kN/m
225 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 10 Premium PTFE-Coated Glass
Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot..
Tear Strength 39.4 kN/m
225 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 10 Tear Resistant PTFE-Coated Glass
Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas..
Tear Strength 39.4 kN/m
225 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 11 Premium PTFE-Coated Glass
Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot..
Tear Strength 39.4 kN/m
225 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 13 Anti-Static PTFE-Coated Glass
Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electri..
Tear Strength 39.4 kN/m
225 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 14 Porous PTFE-Coated Glass
Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas..
Tear Strength 39.5 kN/m
225 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 39.4 kN/m
225 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 39.4 kN/m
225 pli
ASTM D624
Colorite Polymers Vinylbond 6527P-MD Grey 499 Compound
Description: Vinylbond 6527P-MD Grey 499 is a flexible vinyl compound which offers excellent bonding to ABS, low gloss, and low fogging characteristics for use in automotive interior applications. T..
Tear Strength 39.4 kN/m
225 pli
Arlon SQA-TMS-029
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic a..
Tear Strength 39.5 kN/m
225 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 39.5 kN/m
225 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 39.4 kN/m
225 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 10 Primary PTFE-Coated Glass
Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: Ch..
Tear Strength 39.4 kN/m
225 pli
Silicone Property; Arlon SQA-TMS-029
Arlon R36812T010 0.010" Cured Silicone Rubber with Laminated ETFE Film Substrate
Design/Construction:Liner: N/ASide 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorin..
Tear Strength 39.4 kN/m
225 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 10 Porous PTFE-Coated Glass
Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas."..
Copyright © lookpolymers.com All Rights Reserved