Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 38.5 kN/m | 220 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8699 BLK Multi-Flex® A 8699 is a TPE compound based on Kraton G polymer. It is used as medium density acoustic for noise abatement in the auto industry. Multi-Flex TPE contains Kraton™ G.Data provided by.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | ASTM D624 |
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | ASTM D624 |
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ EG-9177 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B65F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible D8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 38.5 kN/m | 220 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Synprene® RT-3870M Styrene Butadiene Block Copolymer (SBC)
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ASTM D624 |
Multibase Multi-Flex® A 7727 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C |
Taiwan PU Corporation UR60 Polyester Urethane Rubber UR60 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die B |
Shin-Etsu Silicones KE-5540U Low Temperature Silicone Elastomer ShinEtsu KE5540 U is a nominal 40 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ASTM D624 |
Teknor Apex Monprene® MP-3955B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 65A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | |
Dow Corning C6-180 ELASTOMER KIT Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | |
Dow Corning C6-350LH ELASTOMER KIT Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | |
Dow Corning SILASTIC® Q7-4565 BIOMEDICAL GRADE ETR ELASTOMER One-part, enhanced tear-resistant silicone elastomers; uncatalyzed (customer selects peroxide catalyst) elastomer materials designed for compounding into elastomer for part fabrication and medical d.. |
|||
Tear Strength | >= 38.6 kN/m | >= 220 pli | Compound Property; ASTM D624 |
Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C; ASTM D624C-73 |
3M SJ-2FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | Die C; ASTM D624C-73 |
3M SJ-3FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3870MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tear Strength | 38.5 kN/m | 220 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 65A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |