Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 256 kN/m | 1460 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible A6DE3 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 256 kN/m | 1460 pli | initiation; ASTM D1004 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Tear Strength | 255 kN/m | 1460 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S375D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 255 kN/m | 1460 pli | ASTM D624 |
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh.. |
|||
Tear Strength | 255 kN/m | 1460 pli | Die C; ASTM D624 |
Lubrizol Estane® S375D Thermoplastic Polyurethane Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tear Strength | 255 kN/m | 1460 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 375D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |