Polymer Property : Tear Strength = 145 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 25.4 kN/m
145 pli
ASTM D624
Multibase Multi-Flex® TPE A 7699 BLK
Multi-Flex® A 7699 is an acoustic barrier compound for medium density applications . Multi-Flex® TPE compounds are based on Shell Kraton G polymers licensed to Multibase. Multi-Flex TPE contains..
Tear Strength 25.4 kN/m
145 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-245A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 25.4 kN/m
145 pli
Initial Tear Strength
Saint-Gobain CHR® 2302-20R UHMW Film Backing Acrylic Adhesive Pressure Sensitive Tape
Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications..
Tear Strength 25.4 kN/m
145 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-4060 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma..