Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 25.2 kN/m | 144 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7020 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 25.3 kN/m | 144 pli | ISO 34 |
Multibase TPSiV® 3111-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc.. |
|||
Tear Strength | 25.2 kN/m | 144 pli | Trouser; ASTM D470 |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |
|||
Tear Strength | 25.2 kN/m | 144 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Tear Strength | 25.2 kN/m | 144 pli | Die B, Silicone Property; ASTM D624 |
Arlon R38095R011 0.011" (0.279 mm) Partially Cross Linked Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Partially Cross Linked Silicone RubberSubstrate: Style 1528 Fiberglass:Side 2: Partially Cross Linked Silicone Rubber Product Use: Electrical InsulationAppearance: Red si.. |