Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 24.0 kN/m | 137 pli | ISO 34-1 |
PolyOne OnFlex™ S HF 50A-3S1981 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | ISO 34-1 |
PolyOne OnFlex™ S KG 70A-3S2019 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tear Strength | >= 24.0 kN/m | >= 137 pli | DIN 53507 |
Karina 651-48/1-BY-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 24.0 kN/m | 137 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ Electro 242-15 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | >= 24.0 kN/m | >= 137 pli | DIN 53507 |
Karina 771-48/1-BY-IS Black PVC Compound Weather resistant PVC compound, recommended for injection and extrusion of automotive profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 24.0 kN/m | 137 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3596/30 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 70 CW Heat Cured Rubber - Cable & Wire Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 60 CW Heat Cured Rubber - Cable & Wire Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | ASTM D624 |
ELASTO UK Dryflex® 500550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | ASTM D624 |
ELASTO UK Dryflex® 502550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | at 25°C |
Daikin DAI-EL LT-302 Fluoroelastomer, Low Temperature Grade, 64% Fluorine Content Features: Flexible up to -30°C, excellent low temperature sealing.Information provided by Daikin Industries. |
|||
Tear Strength | 24.0 kN/m | 137 pli | 73°F, Die C, Across Flow; ASTM D624 |
ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Tear Strength | 24.0 kN/m | 137 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | ASTM D624 |
Arlon T2020-R004 0.020" (0.508 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyethylene Product: Cured Self-Fusing Silicone RubberCross-Secti.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | ISO 34-B |
AlphaGary Evoprene™ 036 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | ISO 34-B |
AlphaGary Evoprene™ 089 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | ISO 34-B |
AlphaGary Evoprene™ Super G 949 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | Die B |
Momentive Performance Materials TSE 2287 Heat Cured Rubber - High Duro Translucent Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 281-64MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tear Strength | 24.0 kN/m | 137 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |