Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 82.4 - 94.7 kN/m | 470 - 540 pli | Average value: 88.2 kN/m Grade Count:3 |
Overview of materials for Silicone Polyurethane, Polycarbonate Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim.. |