Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 2.00 - 113 kN/m | 11.4 - 645 pli | Average value: 24.8 kN/m Grade Count:768 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tear Strength | 73.5 - 113 kN/m | 420 - 644 pli | |
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Tear Strength | 73.5 - 113 kN/m | 420 - 644 pli | |
Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |