Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 98.2 kN/m | 560 pli | Die C; ASTM D624 |
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Buckeye Polymers BP Flex D0853 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |