Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 55.0 kN/m | >= 314 pli | DIN 53507 |
Karina E CAK 85-48/1 Black PVC Compound Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ASTM D624 (die C) |
Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D198K is an aliphatic based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss aspect†on the f.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ASTM D1004 |
SK Chemicals SKYPEL P128DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | DIN 53515 |
Lubrizol ESTANE® T5090 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-A880 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | DIN 53515 |
Lubrizol ESTANE® 5735 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 55.0 kN/m | 314 pli | DIN 53515 |
Lubrizol ESTANE® 58197 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ISO 34 |
Chengdu Polyster FH3303 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H3303 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ASTM D624 |
ELASTO UK Dryflex® 400901S SBS Based Material, 90A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR7060 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | >= 55.0 kN/m | >= 314 pli | ISO 34 |
Austin Novel Materials Texalan® 270A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | >= 55.0 kN/m | >= 314 pli | ISO 34 |
Austin Novel Materials Texalan® 765A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tear Strength | 55.0 kN/m | 314 pli | ASTM D 624 |
API Megol AM DP2395/85 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 55.0 kN/m | 314 pli | DIN ISO 34-1/Bb |
BASF Elastollan 1185 A WM TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tear Strength | >= 55.0 kN/m | >= 314 pli | ISO 34 |
Austin Novel Materials Texalan® 682A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 55.0 kN/m | 314 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | with incision; ISO 34B |
Lubrizol ESTANE® 58214 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 55.0 kN/m | 314 pli | DIN 53515 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 55.0 kN/m | 314 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 55.0 kN/m | 314 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |