Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 53.0 kN/m | 302 pli | B-type, Vulcanized |
KKPC KOSYN 1500 Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 53.0 kN/m | 302 pli | B-type, Vulcanized |
KKPC KOSYN 1500S Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 53.0 kN/m | 302 pli | ASTM D624 |
Sumitomo Chemical ESPOLEX® WT487X Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tear Strength | 53.0 kN/m | 302 pli | ASTM D624 |
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 53.0 kN/m | 302 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 5064-101 TPE, Modified Injection Molding Grade for Auto Mud Flaps The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5064-101 is specifically designe.. |
|||
Tear Strength | 53.0 kN/m | 302 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-40 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 53.0 kN/m | 302 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ DF-19 Woven Fabric 610 Information provided by 3M |
|||
Tear Strength | 53.0 kN/m | 302 pli | without incision; ISO 34B |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |