Polymer Property : Tear Strength = 51.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 51.0 kN/m
291 pli
ASTM D624
Multibase Multi-Flex® TPE A 8000 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 51.0 kN/m
291 pli
ASTM D624
Multibase Multi-Flex® TPE A 8002 BLK
Multi-Flex® TPE 8002 is based on Shell's Kraton G polymer technology and is widely used in the automotive industry for applications requiring elastomeric performance with excellent ozone resistance..
Tear Strength 51.0 kN/m
291 pli
Die B, post cured- 4 hours at 200°C; ASTM D624
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tear Strength 51.0 kN/m
291 pli
ISO 34
Multibase TPSiV® 4100-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-759 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Sulfur
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 51.0 kN/m
291 pli
B-type, Vulcanized
KKPC KOSYN 1502 Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 51.0 kN/m
291 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Sulfur
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 51.0 kN/m
291 pli
ASTM D624
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-759 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 51.0 kN/m
291 pli
GB/T 529
Chengdu Polyster 7502 High Performance Grade TPV
Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 51.0 kN/m
291 pli
ASTM D624
BASF Elastollan® C-60AW Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Tear Strength 51.0 kN/m
291 pli
Warp, Breaking Strength w/o Sizing
3M Nextel™ BF-30 Woven Fabric 440
Information provided by 3M
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 51.0 kN/m
291 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Tear Strength 51.0 kN/m
291 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 51.0 kN/m
291 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex..