Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 50.3 kN/m | 287 pli | ASTM D624 |
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tear Strength | 50.3 kN/m | 287 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-570 Dow-Corning Class VI Elastomer Information provided by Multibase |