Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 50.0 kN/m | 285 pli | Die B, post cured- 8 hours at 200°C; ASTM D624 |
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90037 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | DIN 53507 |
Karina 722-48/1-A-IS Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automobile profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ISO 34B |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ISO 34B |
Huntsman AVALON® 65 AE Thermoplastic Polyurethane Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) LF0250/KJ Low Density Polyethylene LF0250/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: packaging films.Information provid.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ISO 34 |
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE) Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 500850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 502850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 602900S SEBS Based Material, Filled Qualities, 90A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 660900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6 Information provided by EMS Grivory |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® FG 40 NL nat 6021 PA6 Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 off.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6 Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
Colorite Polymers Vinylbond 96-1050-21 BLACK Compound Description: Vinylbond 96-1050-21 BLACK is a flexible vinyl extrusion compound formulated specifically for the window market industry. This particular compound offers excellent bonding characteristi.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN ISO 34-1/Bb |
BASF Elastollan 1185 A W TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | ISO 34 |
Austin Novel Materials Texalan® 370A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | ISO 34 |
Austin Novel Materials Texalan® 570A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tear Strength | 50.0 - 70.0 kN/m | 285 - 399 pli | TM-019K |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-550 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN 53515 |
Lubrizol ESTANE® 54630 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® BM 20 SBG PA* Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good ther.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN ISO 34-1/Bb |
BASF Elastollan B 60 A WHA TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |