Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 46.5 kN/m | 265 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 46.5 kN/m | 265 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified .. |
|||
Tear Strength | 46.5 kN/m | 265 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Basic PTFE-Coated Glass Description: Chemfab® Basic Series products are low resin-content, non-porous, PTFE-coated fiberglass fabrics. Applications are spray shields, separator sheets, release sheets and protective barr.. |
|||
Tear Strength | 46.5 kN/m | 265 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, g.. |
|||
Tear Strength | 46.5 kN/m | 265 pli | |
Dow Corning SILASTIC® LS 5-2060 FLUOROSILICONE RUBBER 60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |