Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® TPE G 7455 BLK Flame retardant thermoplastic rubber based on Shell's Kraton G polymers, manufactured under Shell's license. Product exhibits VO rating. Multi-Flex TPE contains Kraton™ G.Data provided by Multiba.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible A7501 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C8002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible A7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® A 7802 TPE Blk Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® A 8502 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection MoldingExtrusion Uses: Automotive Interior PartsInformation provided by Multiba.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SG03-10(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SG05-10(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SG23-10(R) Primary Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SG26-10(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SGB6-10(R) CHEMLAM Brown Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D1004 |
Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation Tygon S3™ B-44-3, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-ba.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D1004 |
Saint-Gobain Tygon® S3™ B-44-4X I.B. Pressure Tubing Formulation for filling, draining, transfer and processing applications Tygon S3™ B-44-X I.B. tubing, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products... |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 3790 Open Mesh Belting Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® q-GUARD® 215 Insulation Jacketing Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fibergl.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die C; ASTM D624 |
Teknor Apex MF 573 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die C; ASTM D624 |
Teknor Apex Monprene® MP-2264R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Teknor Apex Telcar® TL-2572A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 63A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Diamond Polymers Softflex® 1701-1402 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | >= 43.8 kN/m | >= 250 pli | |
Arlon 10502R125 Cured/Post-cured, Unsupported Silicone Rubber Product Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silic.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 14 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat s.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 1589 PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase |