Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 38.0 kN/m | 217 pli | Type C; ASTM D624 |
LG Chemical LC670 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2752 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-50AB Elastomer KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | ISO 34B |
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, .. |
|||
Tear Strength | 38.0 kN/m | 217 pli | ASTM D624 |
ELASTO UK Dryflex® 600800S SEBS Based Material, Filled Qualities, 80A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 38.0 kN/m | 217 pli | ASTM D624 |
ELASTO UK Dryflex® 602800S SEBS Based Material, Filled Qualities, 80A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 38.0 kN/m | 217 pli | ASTM D624 |
ELASTO UK Dryflex® 660800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | ASTM D624 |
ELASTO UK Dryflex® 662800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | notched; ASTM D624 (C) |
Arkema Group Pebax® 2533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | ISO 34-B |
AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding.. |
|||
Tear Strength | 38.0 - 168 kN/m | 217 - 959 pli | Average value: 91.5 kN/m Grade Count:6 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die B |
Momentive Performance Materials FSE7360 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 38.0 kN/m | 217 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5691 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |