Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 35.0 kN/m | 200 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7204 LC BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 35.0 kN/m | 200 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7521 BLK Ash is 36%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 35.0 kN/m | 200 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8102 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 35.0 kN/m | 200 pli | ISO 34-1 |
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C70UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible R5257A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
Huntsman AVALON® 80 ABX Thermoplastic Polyurethane Introduction: AVALON 80 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 440 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
Karina 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
Karina 65/213 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
Karina 65/225 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2715/50 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
Karina E 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 1040 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE2095-60AB Elastomer KE-2095-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP70AE Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | DIN ISO 34-1/Bb |
BASF Elastoblend LP 9192 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 60 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |