Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection Molding Features:Gloss, LowInformation provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | D624 |
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 212°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 283-40MED Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 60ANS200 Thermoplastic Elastomer
(discontinued **) A soft, translucent thermoplastic elastomer (TPE) with a relative haze of 85 to 90%. This material is shear-dependent and can be processed on conventional thermoplastics equipment for injection mold.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 73°F; ASTM D624 |
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and desig.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL-0153-79 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 60 MP Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-235 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Multibase Multi-Flex® A 5500 MR Natural TPE Thermoplastic Elastomer Information provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® 2915-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® SG33-05(R) Industrial Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 9100-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | |
Dow Corning C6-530 LIQUID SILICONE RUBBER KIT Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and partsInformation provided by Dow Corning |
|||
Tear Strength | 28.0 kN/m | 160 pli | |
ACC MM239 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: ceramic/polyester/PU/epoxy a.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ISO 34-1 |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die B |
Momentive Performance Materials TSE 2277 Heat Cured Rubber - High Duro Translucent Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 38-034M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDiscla.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT38-034 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDi.. |