Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 27.7 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 27.7 kN/m
158 pli
as molded; Die B
Multibase SILASTIC® C7-4535 DICUP R Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 27.7 kN/m
158 pli
ASTM D624 Die B
Freudenberg Simrit S314 Silicone Elastomer (VMQ)
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol..
Tear Strength 27.7 kN/m
158 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 35-HR-9 TPE
Product Description: StarTUFF TF 35-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
Tear Strength 27.7 kN/m
158 pli
Dow Corning SILASTIC® LS 4-9038 FLUOROSILICONE RUBBER
50 Durometer, off-white, uncatalysed, high temperature grade fluorosilicone base.Information provided by Dow Corning
Copyright © lookpolymers.com All Rights Reserved