Polymer Property : Tear Strength = 23.5 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 23.5 kN/m
134 pli
ASTM D624
Polymax® Maxelast® P2950T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tear Strength 23.5 kN/m
134 pli
Split; ASTM D624
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Tear Strength 23.5 kN/m
134 pli
Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/30 Polyurethane Casting Elastomer
Compound of CPU-69-A/B with a mixing ratio of 100/30Information provided by Taiwan PU Corporation.MatWeb has a separate entry for the unmixed A nd B components.
Tear Strength 23.5 kN/m
134 pli
at 25°C
Daikin DAI-EL G-702 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent elongation and tear strength.Informatio..
Tear Strength 23.5 kN/m
134 pli
at 25°C
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries.
Tear Strength 23.5 kN/m
134 pli
at 25°C
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin ..
Tear Strength 23.5 kN/m
134 pli
Fill, Breaking Strength w/o Sizing
3M Nextel™ AF-11 Industrial Woven Fabric 312
Information provided by 3M
Tear Strength 23.5 kN/m
134 pli
Fill, Breaking Strength w/o Sizing
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
Tear Strength 23.5 kN/m
134 pli
Fill, Breaking Strength w/o Sizing
3M Nextel™ AF-14 Industrial Woven Fabric 312
Information provided by 3M