Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 17.7 kN/m | 101 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Tear Strength | 17.7 kN/m | 101 pli | ASTM D624 Die B |
Freudenberg Simrit S50 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |
|||
Tear Strength | 17.7 kN/m | 101 pli | 500 mm/min; ASTM D 624 |
Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, .. |
|||
Tear Strength | 17.7 kN/m | 101 pli | [ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us.. |