Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.4 kN/m | 87.9 pli | Infiltrated with flexseal (8-dip process); ASTM D624 |
Proto3000 Duraform® Flex Selective Laser Sintering (SLS®) Prototyping Polymer Description: Thermoplastic elastomer material with rubber-like flexibility and functionality.DuraForm FlexSeal Infiltration:FlexSeal fluid infiltration is an easy-to-use method of coloring, strength.. |
|||
Tear Strength | 15.4 kN/m | 88.0 pli | Die B |
Shin-Etsu Silicones SV-15000U Silicone Rubber SV15000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat.. |
|||
Tear Strength | 15.4 kN/m | 88.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 45-1000 TPE Product Description: StarGrip GP 45-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |