Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.0 kN/m | 85.6 pli | D624 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2735/30 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Karina CAK 65-48/1-F Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Karina E 4048/1-TRE Kariprene Black Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials HV 3/506 Heat Cured Rubber - High Temperature Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B500 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg Z900 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B600 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ASTM D624 |
ELASTO UK Dryflex® 660400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ASTM D624 |
ELASTO UK Dryflex® 660450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ASTM D624 |
ELASTO UK Dryflex® 662450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8014-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
ACC MM240T Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: rapid prototyping. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg Commercial Neoprene® C433 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 15.0 - 55.0 kN/m | 85.6 - 314 pli | Average value: 28.5 kN/m Grade Count:19 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |