Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 149 kN/m | 850 pli | At 73°F; ASTM D624 |
DuPont Bexloy® AXW504BK Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Tear Strength | 149 kN/m | 850 pli | At 73°F; ASTM D624 |
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Tear Strength | 149 kN/m | 850 pli | |
Dow Pellethane® 2354-55D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-55D is elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyureth.. |