Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 14.0 kN/m | 80.0 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 281-45MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FFSL 7031 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tear Strength | 14.0 kN/m | 80.1 pli | ASTM D624, Die C |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tear Strength | 14.0 kN/m | 80.0 pli | Initial Tear Strength |
Saint-Gobain CHR® SG55-03(R) Anti-Static Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 14.0 kN/m | 80.0 pli | Initial Tear Strength; ASTM D624 |
Saint-Gobain COHRlastic® 9040 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tear Strength | 14.0 kN/m | 80.0 pli | |
Dow Corning SILASTIC® M-3 RTV SILICONE RUBBER BASE & CURING AGENT Dow Corning Silastic® M-3 RTV Silicone Rubber is an addition cured (platinum catalyzed); high durometer silicone rubber developed for use in prototyping, architectural, and furniture applications w.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
ELASTO UK Dryflex® 600300S SEBS Based Material, Filled Qualities, 30A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
ELASTO UK Dryflex® 602300S SEBS Based Material, Filled Qualities, 30A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
ELASTO UK Dryflex® 660300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | |
ACC MM906 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tear Strength | 14.0 - 35.0 kN/m | 79.9 - 200 pli | ASTM D 624 |
API Megol AM DP1741 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 14.0 kN/m | 80.0 pli | Silicone Property; ASTM D624 |
Arlon 47571R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone Rubber Substrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicone gum on fibergl.. |
|||
Tear Strength | 14.0 kN/m | 80.0 pli | Silicone Property; ASTM D624 |
Arlon 47571R012 0.012" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEThis data represents typical values for the produ.. |