Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0080442 GPa @Temperature 1450 °C, Time 10800 sec |
1.1667 ksi @Temperature 2640 °F, Time 3.00 hour |
|
Chosun Refractories AU3 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |